±0.1°
Achievable angle on a controlled bend. Cumulative angle across several bends is stated separately.
Request a quote ↗CNC BENDING
Press-brake forming to the approved geometry. The sequence is planned so a bend is never blocked by one already made, and the bend allowance is confirmed on the first-off rather than assumed from a table.
±0.1° on angle · 3,000 mm · 1 piece

FORMING CAPACITY
Bending is where a design that cuts perfectly turns out to be impossible. These four numbers cover most of the reasons.
Achievable angle on a controlled bend. Cumulative angle across several bends is stated separately.
Longest bend in one pass. Longer panels are formed in two setups with the joint in the middle.
Working thickness. Above 6 mm the tool radius has to rise with the thickness or the outside face cracks.
No tooling charge. Standard tooling covers most work; a special tool is quoted only where geometry demands it.
HOW A BEND IS SPECIFIED
Two panels can measure the same on the flat pattern and come out different once bent. These are the parameters responsible.
The inside radius should be at least equal to the material thickness. Tighter than that and the outside face stretches beyond what the material will take, which shows up as a hairline crack along the bend — often not until after coating.
The flat pattern is not the sum of the outside dimensions. Material stretches through the bend, and the allowance depends on the radius, the thickness and the tooling. It is calculated, then confirmed on the first-off rather than trusted blindly.
A bend that stops in the middle of a panel tears at the end of the bend line unless a notch is cut there. It is a small detail on the drawing and a visible defect without it.
A bent leg shorter than the tooling opening cannot be formed — the tool cannot reach it without the tooling fouling the panel. Light-gauge work gets down to roughly four times the thickness; heavier work needs more.
Where several bends meet, the order decides whether the last one is reachable. This is planned before the first bend is made, not discovered halfway through a batch.
Every material returns slightly after the tool lifts. Stainless returns more than mild steel and aluminium more again, so the same tooling setting does not produce the same angle across grades. The control compensates, and the first-off confirms it.
A hole placed close to a bend line distorts into an oval as the material stretches. Keep it at least 2.5 times the thickness away from the inside of the bend, or add a notch.
The brushed or coated face has a direction. Which side faces out on each bend is stated on the drawing, or the brush direction ends up running two ways on one panel.
FROM FILE TO FINISHED PANEL
Each step produces something that can be checked before the next one starts, which is what stops a tooling problem becoming a batch of scrap.
01
The formed part is unfolded to a flat layout with the bend allowance applied. This file is what the laser cuts, so an error here is an error in every panel that follows.
02
Upper and lower tooling are chosen for the radius, the angle and the bend leg lengths involved. A radius that needs a tool we do not hold is quoted before the order, not after.
03
The first part off the setup is measured for angle and bend leg length against the approved drawing. Springback is corrected here, on one part, instead of on a batch.
04
The run follows the confirmed setting. Angle is checked at intervals through the batch, not only at the start, because tooling temperature and material batch both drift slowly.
WHY STAINLESS IS DIFFERENT
Stainless steel work-hardens as it forms and springs back further than mild steel. An angle that measures correctly in carbon steel will come off the same tooling open by a degree or more in 304.
That is not a reason to avoid stainless — it is a reason to confirm the allowance on the first part of each grade rather than carrying a setting across from the last job. Which is what the first-off step exists for.
It also matters for aluminium, which returns less predictably still and marks easily against steel tooling. Where the visible face cannot carry a tooling mark, protective tape goes on before forming and comes off before coating.

NEXT STEP
Send the formed model and the bend leg lengths. We will say whether the geometry forms cleanly and what it needs if not.
SEND DRAWINGS
Share the drawings or the dimensions you have. Engineering reviews them and returns the findings with the quotation — usually within one working day.